The hardener for fiberglass resin is methyl ethyl keytone peroxide it
reacts with the cobalt in the resin.
I have no idea of what that would do on a circuit board. I do know however,
that fiberglass panels work well as insulators.
, Having built boats for 18 years , I have some large panels (cutouts from
building boats) that I use at the feed point, for (multi wire) parallel
dipoles.
FRP- fiberglass reinforced plastic ..makes a good insulator and it
extremely strong.