2 or 3% silver is added to tin-lead solder to prevent leaching of gold
or silver terminations from certain surface mount components (and the
terminal strips in very old Tektronix scopes). These components are
often used for hybrid circuits, but solder-coated terminations seem a
lot more common for components intended for PCB use. I haven't seen a
leaching problem with the solder-coated terminations using ordinary
tin-lead solder.

Is there some other advantage of a 2 or 3% silver addition?

Roy Lewallen, W7EL

Dave Platt wrote:
. . .


I tend to prefer the eutectic, or a eutectic modified with 2% silver.

 
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
Warning -- bad new type of solder flux Mike Knudsen Boatanchors 20 March 31st 04 11:46 PM
sn96.3 ag3.7 solder qstn BOEING377 Boatanchors 12 February 17th 04 06:04 AM
FS: SOLDER REWORK STATION dt Equipment 0 December 7th 03 06:25 PM
FS: SOLDER REWORK STATION dt Equipment 0 December 7th 03 06:25 PM
AMBULANCE CHASER Have You Been Harmed By Lead Solder? radioranch Equipment 5 July 8th 03 10:46 PM


All times are GMT +1. The time now is 05:20 PM.

Powered by vBulletin® Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright ©2004-2025 RadioBanter.
The comments are property of their posters.
 

About Us

"It's about Radio"

 

Copyright © 2017